The Oil-based Coloring Agent product could be easily applied in two main steps to achieve a pretty color viewing. The good permeability allows color to penetrate deep down into surface, and enables the coloring be long-lasting.

1. Preparing the surface

·To the hard surface that is above C30 or to the silicon carbide surface, grinding and cleaning the surface with water to 300-grit. Then allow the surface to dry.

·To the loosen surface, which had not been hardened and could not be grinded, it should be firstly hardened by C/A hardening agents (See Manual of C/A hardening agent for detail) and then be grinded to 300~500-grit. Cleaning the surface with water and leaving it to dry.

·To the surface that is in the middle of above, it could be treated with agent A for one time, and then be grinded to 300~500-grit. Cleaning and drying the surface for the next step.

 

The first step includes the treatments of hardening, grinding, cleaning and drying. When the preparation is over, the surface should be ready for coloring. The prepared surface has good fineness and is sufficiently dry. It is not over-hardened that the coloring agent might penetrate poorly, neither over-loosen, which will shorten the service life.  The oil-base agent is more easier to penetrate into surface compared to water-base agent, therefore the surface can be grinded more finer. However, it is also important, that the surface need to be dry and fine before coloring.

 

2. Coloring

1.Before start coloring, be sure that the surface is (1) sufficiently dry, and (2) finely grinded.

2.Decide a coloring method either (1) spraying, or (2) using cotton mop to spread.

3.Coloring the first layer on surface for the first time. If the coloring agent is not painted evenly, or the color is light, should add more by mopping or spraying.

4.Apply the second coloring layer when the first layer is dry. The time between should not be less than 4 hours.

5.When the second coloring layer is completely dry, use lapping machined to polish and remove residuals (The accompanied sponge grit disk should be higher than 3000-grit). The surface should be polished twice in horizontal and vertical directions. At last, remove the dust by clean, dry mop.

 

 

3. Color fixing

1.Spray the color-fixing agent, afterwards dropping water on the surface.

2.When the surface is dry, dry-polish with 1000 to 2000-grit till the surface is fine. (Do not polish with water)

3.Wash the surface by scrubber with white pad in water.

4.Once the surface dries, apply the Lightening Agent on the surface (See the manual of Lightening Agent ) and polish 1 to 3 times by high-speed polishing machine equipped by 3# pad.

 

Attention: The surface should not contact with water after the coloring and crosslinking steps, but only when the coloring-fixing step completes.